关于挠性线路板油墨印刷的专业术语,下面的这段英语如何翻译,谢谢!Polyester mesh counts from 86 to 150 counts per inch should be used. Screen tension should be uniform and a minimum of 30 N/cm2. Squeegee Shore hardness should

来源:学生作业帮助网 编辑:作业帮 时间:2024/11/17 23:58:28

关于挠性线路板油墨印刷的专业术语,下面的这段英语如何翻译,谢谢!Polyester mesh counts from 86 to 150 counts per inch should be used. Screen tension should be uniform and a minimum of 30 N/cm2. Squeegee Shore hardness should
关于挠性线路板油墨印刷的专业术语,下面的这段英语如何翻译,谢谢!
Polyester mesh counts from 86 to 150 counts per inch should be used. Screen tension should be uniform and a minimum of 30 N/cm2. Squeegee Shore hardness should be 65-70 durometer. Flood /print sequencing should be used to ensure adequate fill between circuitry.

关于挠性线路板油墨印刷的专业术语,下面的这段英语如何翻译,谢谢!Polyester mesh counts from 86 to 150 counts per inch should be used. Screen tension should be uniform and a minimum of 30 N/cm2. Squeegee Shore hardness should
应使用目数(点数)为每英寸从86到150的聚酯网.筛子张力须均匀,最少30 牛/ cm2.橡胶滚轴以硬度计测试应为肖氏硬度65-70.须使用充注/印刷排序,以确保线路间有充足的填充.